Interlayer separation
Interlayer separation

Cause 1: Leveling

platform and screen leveling four corners are not level or too far away, should be re-leveling, A4 paper from all corners of the draw resistance consistent

Cause 2: Light source

part of the light source is not uniform light, which may lead to inconsistent degree of exposure in different areas

Cause 3: Cutting

exposure time is not enough, the layers are not fully cured, resulting in separation, layer thickness and exposure does not correspond, such as 0.1mm layer thickness using 0.025mm layer thickness exposure parameters, separation occurs, should be appropriate to increase the exposure time; lifting speed is faster, the separation force is greater resulting in separation; less support or thin, the top surface can not be fully supported, resulting in partial print failure, separation between layers

Cause 4: Temperature

the temperature is too low without insulation, resin activity is low, it is recommended to open the air conditioning 25-35 ℃ printing